In normal production, the China Micronized Pe Wax near me can be directly added to polyolefin as an additive, and has excellent cold resistance, heat resistance, chemical resistance and abrasion resistance. In the production process of the China micronized PE Wax, controlling the pyrolysis temperature and time is an important factor to ensure the properties and quality of the pyrolysis wax.

The high temperature cracking of the China micronized PE WAX near me requires more than three hundred degrees Celsius. If the temperature is too low, it will easily lead to incomplete degradation, insufficient molecular chain breakage, and poor product fluidity, which is not conducive to various processing applications. If the cracking temperature of the China micronized PE wax is too high, it is easy to cause excessive power consumption, increased production cost, too fast fluidity, large cooling time and too fast discharge, and it is easy to cause combustion and cause accidents.
In addition, the discharge circulation cooling system of the China micronized PE wax near me should be perfect, and the discharge temperature should be controlled below eight hundred degrees Celsius. If the cooling effect of the device is not good, the micronized PE wax is exposed to high temperature in the air and is easily oxidized, and the product is gray, which is not conducive to use.

Product Categories

Home

Product

Whatsapp

About Us

Inquiry

We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

Send